产品名称

INCONEL 22

没有此类产品
产品描述
By virtue of its contents of chromium, molybdenum, tungsten and controlled iron, this alloy exhibits excellent resistance to both oxidizing and reducing acid environments, as well as those containing mixed acids. It is particularly useful for resistance to pitting and crevice corrosion in acid-halide environments. Applications include the chemical processing, pollution control, flue gas desulfurization, waste incineration and pulp and paper processing industries.
STANDARD PRODUCT FORMS
Sheet, strip, plate, round bar, flat bar, forging stock,
hexagon and wire.
MAJOR SPECIFICATIONS
USN N06022
ASTM B 366, B 462, B 564, B 574,
B 575, B 619, B 622, B 626,
B 751, B 775, B 829, B 906
ASME SB-366, SB-564, SB-574,
SB-575, SB-619, SB-622,
SB-626, SB-751, SB-775,
SB-829, SB-906
ASME Code Cases 2226,
N-621
Werkstoff Nr. 2.4602
ISO 6207, 6208, 9723,
9724
DIN 17744, 17750-17754
LIMITING CHEMICAL COMPOSITION, %
Ni........Remainder
Cr......20.0 – 22.5
Mo.....12.5 – 14.5
Fe...........2.0 – 6.0
W............2.5 – 3.5
Co........... 2.5 max.
C........ 0.015 max.
Mn........0.50 max.
V...........0.35 max.
S...........0.02 max.
Si..........0.08 max.
P...........0.02 max.
PHYSICAL CONSTANTS AND THERMAL PROPERTIES
Density, Ib/in3 (g/cm3)............................................0.311 (8.61)
Melting Range, °F (°C)..............2464 – 2529 (1351 – 1387)
Specific Heat, Btu/lb•°F (J/kg•°C).......................0.091 (381)
Curie Temperature, °F (°C)................................. <-320 (-196)
Permeability at 200 Oersted (15.9 kA/m).................. <1.001
Coefficient of Expansion, 10-6 in/in•°F (μm/m•°C)
70-200°F (21–93°C)...................6.90 (12.42)
70-1000°F (21–538°C).............. 7.46 (13.43)
70-1800°F (21–982°C).............. 7.84 (14.11)
Thermal ConductivityA, Btu•in/ft2•h•°F (W/m•°C)........91 (13.2)
Electrical ResistivityA, ohm•circ mil/ft (μΩ•m).... 730.7 (1.215)
Young’s ModulusA, 106 psi (GPa)............................ 30.3 (209)
Shear’s ModulusA, 106 psi (GPa)............................ 11.0 (75.8)
Poisson’s RatioA....................................................................... 0.30
HardnessA, HRB...........................................................................86
ARoom temperature, as aged.
TYPICAL MECHANICAL PROPERTIES
INCONEL  22
Corresponding parameter set not found, please add it in property template of background
暂未实现,敬请期待
暂未实现,敬请期待
Previous article
Next article

Product