INCONEL N06230
产品描述
A carbide strengthened nickel-chromiumtungsten alloy with an exceptional combination of strength, stability and resistance to corrosion at very high temperatures. Alloy N06230 offers particularly good resistance to oxidation at temperatures greater than 1800°F (980°C). It also offers good resistance to carburization and nitridation. Potential applications for this alloy include equipment and components for landbased gas turbines, thermal and petrochemical processing, heat treating, and ore refining.
STANDARD PRODUCT FORMS
Contact Special Metals.
MAJOR SPECIFICATIONS
UNS N06230
W. Nr. 2.4733
ASTM B 366, B 435, B 564,
B 572, B 619, B 622, B 626
ASME SB 435, SB 564,
SB 572, SB 619,
SB 622, SB 626
SAE/AMS 5839, 5878, 5891
W. Nr. 2.4733
ASTM B 366, B 435, B 564,
B 572, B 619, B 622, B 626
ASME SB 435, SB 564,
SB 572, SB 619,
SB 622, SB 626
SAE/AMS 5839, 5878, 5891
LIMITING CHEMICAL COMPOSITION, %
Ni........Remainder
Fe........... 3.0 max.
Cr......20.0 – 24.0
Co........... 5.0 max.
Mo..........1.0 – 3.0
W.......13.0 – 15.0
C........0.05 – 0.15
Si.......0.25 – 0.75
Mn.....0.30 – 1.00
P........ 0.030 max.
S........ 0.015 max.
Al........0.20 – 0.50
La... 0.005 – 0.050
B........ 0.015 max.
Fe........... 3.0 max.
Cr......20.0 – 24.0
Co........... 5.0 max.
Mo..........1.0 – 3.0
W.......13.0 – 15.0
C........0.05 – 0.15
Si.......0.25 – 0.75
Mn.....0.30 – 1.00
P........ 0.030 max.
S........ 0.015 max.
Al........0.20 – 0.50
La... 0.005 – 0.050
B........ 0.015 max.
PHYSICAL CONSTANTS AND THERMAL PROPERTIES
Density, Ib/in3..........................................................................0.322
g/cm3......................................................................... 8.91
Melting Point, °F......................................................2480 – 2570
°C......................................................1360 – 1410
Permeability at 200 Oersted (15.9 kA/m).....................1.002
Coefficient of Expansion, 70 – 600°F, 10-6 in/in •°F...........6.9
20 – 316°C, 10-6 cm/cm•°C....12.4
Electrical Resistivity, ohm • circ mil/ft.............................. 759
μΩ•m.................................................. 126
Young's Modulus, 103 ksi...................................................... 30.7
GPa............................................................ 211
Shear Modulus, 103 ksi.......................................................... 11.4
GPa............................................................... 78.8
Poisson's Ratio........................................................................ 0.34
g/cm3......................................................................... 8.91
Melting Point, °F......................................................2480 – 2570
°C......................................................1360 – 1410
Permeability at 200 Oersted (15.9 kA/m).....................1.002
Coefficient of Expansion, 70 – 600°F, 10-6 in/in •°F...........6.9
20 – 316°C, 10-6 cm/cm•°C....12.4
Electrical Resistivity, ohm • circ mil/ft.............................. 759
μΩ•m.................................................. 126
Young's Modulus, 103 ksi...................................................... 30.7
GPa............................................................ 211
Shear Modulus, 103 ksi.......................................................... 11.4
GPa............................................................... 78.8
Poisson's Ratio........................................................................ 0.34
TYPICAL MECHANICAL PROPERTIES