Hotline Tel
021-69925077
Mobile: +86 139 1729 0748
Tel: +86 21 6992 2027
Fax: +86 21 6992 5075
Email: jack@ksalloy.com
Add: 5999 Huyi Highway, Shanghai, China
COPYRIGHT © 2018 Shanghai Kangsheng Aerospace Technology Co., Ltd 沪ICP备10214040号
Page view:
产品名称
INCOLOY 28
产品描述
INCOLOY 28 (UNS N08028) is a highly corrosion-resistant austenitic alloy offering resistance to a variety of media. The alloy resists attack in reducing media due to its contents of nickel, copper and molybdenum and is resistant to oxidizing species due to its high level of chromium. Alloy 28 offers resistance to general, localized and stress-induced corrosion by chlorides and hydrogen sulfides. Thus, it is widely used in oilfield applications. Tubes are cold worked to high levels of strength for downhole service in deep sour gas wells. With its excellent combination of strength and corrosion resistance, alloy 28 also finds applications in the process industries. It is especially useful for handling phosphoric acid. Due to its resistance to chlorides, alloy 28 tubes may be used in the marine industry for seawater-cooled heat exchangers.
STANDARD PRODUCT FORMS
Tube.
MAJOR SPECIFICATIONS
UNS N08028
ASTM B 668, B 709, B 829
ASME SB-668, SB-709, SB-829
Werkstoff Nr. 1.4563
NACE MR-01-75
ASTM B 668, B 709, B 829
ASME SB-668, SB-709, SB-829
Werkstoff Nr. 1.4563
NACE MR-01-75
LIMITING CHEMICAL COMPOSITION, %
Ni ......30.0 – 34.0
Cr.......26.0 – 28.0
Mo..........3.0 – 4.0
Cu..........0.6 – 1.4
Fe............ Balance
Mn........2.50 max.
C........ 0.030 max.
P......... 0.030 max.
S........ 0.030 max.
Si..........1.00 max.
PHYSICAL CONSTANTS AND THERMAL PROPERTIES
Density, Ib/in3 (g/cm3).................................................0.29 (8.0)
Specific Heat, Btu/lb•°F (J/kg•°C)......................0.105 (450)
Coefficient of Expansion, 10-6 in/in•°F (μm/m•°C)
75-200°F (21-93°C).........................8.3 (15.0)
75-500°F (21-260°C)......................8.8 (15.9)
75-800°F (21-427°C)......................9.3 (16.8)
Thermal ConductivityA, Btu • in/ft2•h•°F.............................66
W/m •°C......................................... 11.4
Electrical ResistivityA, ohm •circ mil/ft (μΩ•m)..... 594 (0.99)
Young's ModulusA, 106 psi (GPa)............................ 29.0 (200)
ARoom temperature, as annealed.
Specific Heat, Btu/lb•°F (J/kg•°C)......................0.105 (450)
Coefficient of Expansion, 10-6 in/in•°F (μm/m•°C)
75-200°F (21-93°C).........................8.3 (15.0)
75-500°F (21-260°C)......................8.8 (15.9)
75-800°F (21-427°C)......................9.3 (16.8)
Thermal ConductivityA, Btu • in/ft2•h•°F.............................66
W/m •°C......................................... 11.4
Electrical ResistivityA, ohm •circ mil/ft (μΩ•m)..... 594 (0.99)
Young's ModulusA, 106 psi (GPa)............................ 29.0 (200)
ARoom temperature, as annealed.
TYPICAL MECHANICAL PROPERTIES