产品名称
INCOLOY 25-6HN
产品描述
INCOLOY alloy 25-6HN is a super-austenitic stainless steel containing 6% molybdenum with properties enhanced by its content of nitrogen. Its high content of nickel results in thermal stability and resistance to stress corrosion cracking. Designated as UNS N08367, alloy 25-6HN directly competes with alloy AL6XN®1. The same ASTM, ASME and NACE specifications cover the alloys. Alloy 25-6HN offers significantly improved strength and corrosion resistance in most environments over conventional austenitic stainless steels such as AISI 304 or 316L. Typical applications include welded tubes for heat exchangers for both chemical processing and marine applications and for desalination systems, flue gas desulfurization equipment for coal-fired power plants and reaction vessels for pharmaceutical production. 1“AL6XN” is a registered trademark of Allegheny Ludlum Corporation.
STANDARD PRODUCT FORMS
Sheet, strip, plate, round bar, wire rod and forging stock.
MAJOR SPECIFICATIONS
UNS N08367
ASTM B688, A240, B691, B564,
B472, B676, B675, B804,
B462, B366
ASME SB688, SA240, SB691,
SB564, SB472, SB676,
SB675, SB804, SB462,
SB366
ASTM B688, A240, B691, B564,
B472, B676, B675, B804,
B462, B366
ASME SB688, SA240, SB691,
SB564, SB472, SB676,
SB675, SB804, SB462,
SB366
LIMITING CHEMICAL COMPOSITION, %
Ni.....23.50–25.50
Cr....20.00–22.00
Fe............Balance
Mo........6.00–7.00
N.......... 0.18–0.25
Cu........0.75 max.
C...........0.03 max.
Mn.........2.00 max
Si..........1.00 max.
P......... 0.040 max.
S........ 0.030 max.
PHYSICAL CONSTANTS AND THERMAL PROPERTIES
Density, Ib/in3.........................................................................0.291
g/cm3......................................................................... 8.06
Melting Range, °F...................................................2470 – 2550
°C...................................................1320 – 1400
Permeability at 200 Oersted.............................................1.003
Coefficient of Expansion, 10-6 in/in •°F
70 – 200°F..................................................... 8.66
70 – 800°F .................................................... 9.05
70 – 1200°F ................................................. 9.53
g/cm3......................................................................... 8.06
Melting Range, °F...................................................2470 – 2550
°C...................................................1320 – 1400
Permeability at 200 Oersted.............................................1.003
Coefficient of Expansion, 10-6 in/in •°F
70 – 200°F..................................................... 8.66
70 – 800°F .................................................... 9.05
70 – 1200°F ................................................. 9.53
TYPICAL MECHANICAL PROPERTIES