产品名称
INCONEL 600
产品描述
A nickel-chromium alloy with good oxidation resistance at high temperatures and resistance to chloride-ion stress-corrosion cracking, corrosion by high-purity water and caustic corrosion. Used for furnace components, chemical and food processing,nuclear engineering and sparking electrodes.
STANDARD PRODUCT FORMS
Pipe, tube, sheet, strip, plate, round bar, flat bar, forging
stock, hexagon, wire and extruded section.
stock, hexagon, wire and extruded section.
MAJOR SPECIFICATIONS
UNS N06600
BS 3072 – 3076 (NA14)
ASTM B 163, B 166 – B 168,
B 366, B 516, B 517, B 564,
B 751, B 775, B 829
ASME SB-163, SB-166 – SB-168,
SB-366, SB-516, SB-517,
SB-564, SB-751, SB-775,
SB-829
ASME Code Cases 1827, N-20,
N-253, N-576
SAE AMS 5540, 5580,
5665, 5687
DIN 17742, 17750 – 17754
Werkstoff Nr. 2.4816
VdTÜV 305
NACE MR-01-75
QQ-W 390
EN 10095
ISO 6207, 6208, 9723 –9725,
4955A
BS 3072 – 3076 (NA14)
ASTM B 163, B 166 – B 168,
B 366, B 516, B 517, B 564,
B 751, B 775, B 829
ASME SB-163, SB-166 – SB-168,
SB-366, SB-516, SB-517,
SB-564, SB-751, SB-775,
SB-829
ASME Code Cases 1827, N-20,
N-253, N-576
SAE AMS 5540, 5580,
5665, 5687
DIN 17742, 17750 – 17754
Werkstoff Nr. 2.4816
VdTÜV 305
NACE MR-01-75
QQ-W 390
EN 10095
ISO 6207, 6208, 9723 –9725,
4955A
LIMITING CHEMICAL COMPOSITION, %
Nia.........72.0 min.
Cr...... 14.0 – 17.0
Fe........ 6.0 – 10.0
aPlus Co.
C...........0.15 max.
Mn.......... 1.0 max.
S........ 0.015 max.
Si............ 0.5 max.
Cu.......... 0.5 max.
Cr...... 14.0 – 17.0
Fe........ 6.0 – 10.0
aPlus Co.
C...........0.15 max.
Mn.......... 1.0 max.
S........ 0.015 max.
Si............ 0.5 max.
Cu.......... 0.5 max.
PHYSICAL CONSTANTS AND THERMAL PROPERTIES
Density, Ib/in3.........................................................................0.306
g/cm3......................................................................... 8.47
Melting Range, °F....................................................2470 – 2575
°C....................................................1354 – 1413
Specific Heat, Btu/lb•°F.....................................................0.106
J/kg•°C............................................................ 444
Curie Temperature, °F.......................................................... -192
°C.......................................................... -124
Permeability at 200 Oersted (15.9 kA/m).....................1.010
Coefficient of Expansion, 70 – 200°F, 10-6 in/in •°F........ 7.4
21 – 93°C, μm/m •°C............. 13.3
Thermal Conductivity, Btu • in/ft2•h•°F............................ 103
W/m •°C........................................... 14.9
Electrical Resistivity, ohm •circ mil/ft................................ 620
μΩ•m................................................. 1.03
g/cm3......................................................................... 8.47
Melting Range, °F....................................................2470 – 2575
°C....................................................1354 – 1413
Specific Heat, Btu/lb•°F.....................................................0.106
J/kg•°C............................................................ 444
Curie Temperature, °F.......................................................... -192
°C.......................................................... -124
Permeability at 200 Oersted (15.9 kA/m).....................1.010
Coefficient of Expansion, 70 – 200°F, 10-6 in/in •°F........ 7.4
21 – 93°C, μm/m •°C............. 13.3
Thermal Conductivity, Btu • in/ft2•h•°F............................ 103
W/m •°C........................................... 14.9
Electrical Resistivity, ohm •circ mil/ft................................ 620
μΩ•m................................................. 1.03
TYPICAL MECHANICAL PROPERTIES