INCONEL 601

没有此类产品
产品描述
A nickel-chromium alloy with an addition of aluminum for outstanding resistance to oxidation and other forms of high-temperature corrosion.It also has high mechanical properties at elevated temperatures. Used for industrial furnaces;heat-treating equipment such as baskets, muffles,and retorts; petrochemical and other process equipment; and gas-turbine components.
STANDARD PRODUCT FORMS
Pipe, tube, sheet, strip, plate, round bar, flat bar, forging
stock, hexagon and wire.
MAJOR SPECIFICATIONS
UNS N06601
ASTM B 166 – B 168, B 751,
B 775, B 829
ASME SB-166 – SB-168,
SB-751, SB-775, SB-829
ASME Code Case 1500
DIN 17742, 17750 – 17754
Werkstoff Nr. 2.4851
EN 10095
ISO 6207, 6208, 9723-9725
LIMITING CHEMICAL COMPOSITION, %
Ni.......58.0 – 63.0
Cr.......21.0 – 25.0
Al............1.0 – 1.7
Fe.......Remainder
C...........0.10 max.
Mn.......... 1.0 max.
Si..........0.50 max.
S........ 0.015 max.
Cu.......... 1.0 max.
PHYSICAL CONSTANTS AND THERMAL PROPERTIES
Density, Ib/in3.........................................................................0.293
g/cm3......................................................................... 8.11
Melting Range, °F....................................................2480 – 2571
°C......................................................1360-1411
Specific Heat, Btu/lb•°F.....................................................0.107
J/kg•°C............................................................ 448
Curie Temperature, °F........................................................<-320
°C........................................................<-196
Permeability at 200 Oersted (15.9 kA/m).....................1.003
Coefficient of Expansion, 70 – 200°F, 10-6 in/in •°F......7.60
20 – 100°C, μm/m •°C........13.75
Thermal Conductivity, Btu • in/ft2•h•°F...............................78
W/m •°C........................................... 11.2
Electrical Resistivity, ohm •circ mil/ft................................ 717
μΩ•m................................................. 1.19
TYPICAL MECHANICAL PROPERTIES
INCONEL 601
Corresponding parameter set not found, please add it in property template of background
暂未实现,敬请期待
暂未实现,敬请期待
Previous article
Next article

Product