产品名称
FERRY ALLOY
产品描述
A copper-nickel alloy used mainly for its electrical properties. It has mediumrange electrical resistivity and a very low temperature coefficient of resistance (TCR). The low TCR makes the alloy useful for wire-wound precision resistors having operating temperatures up to 750°F (400°C). A reproducible electromotive force against copper makes the alloy suitable for thermocouples and thermocouple compensating leads.
STANDARD PRODUCT FORMS
Strip and wire.
MAJOR SPECIFICATIONS
ASTM B 267, DIN 17644, Werkstoff Nr. 2.0842
LIMITING CHEMICAL COMPOSITION, %
Limiting
Ni .......Remainder
Cu.................55.0 a
a Nominal
Fe ..........1.0 max.
C ............0.1 max.
Mn .........1.0 max.
Si ...........0.5 max.
Ni .......Remainder
Cu.................55.0 a
a Nominal
Fe ..........1.0 max.
C ............0.1 max.
Mn .........1.0 max.
Si ...........0.5 max.
PHYSICAL CONSTANTS AND THERMAL PROPERTIES
Density, Ib/in3 ........................................................................0.321
g/cm3 .........................................................................8.89
Melting Range, °F ...................................................2230 – 2320
°C ...................................................1220 – 1270
Specific Heat, Btu/lb • °F ....................................................0.094
J/kg • °C ...........................................................394
Temp. Coefficient of Resistance
68 – 212°F, 10-6 ohm/ohm • °F................17
20 – 100°C, µ Ω/Ω• °C ..................................30
Coefficient of Expansion, 68 – 212°F, 10-6 in/in • °F.....8.17
20 – 100°C, µm/m • °C .........14.7
Thermal Conductivity, Btu • in/ft2 • h • °F ...........................155
W/m • °C ..........................................22.4
Electrical Resistivity, ohm • circ mil/ft ...............................295
µ Ω• m ..............................................0.490
g/cm3 .........................................................................8.89
Melting Range, °F ...................................................2230 – 2320
°C ...................................................1220 – 1270
Specific Heat, Btu/lb • °F ....................................................0.094
J/kg • °C ...........................................................394
Temp. Coefficient of Resistance
68 – 212°F, 10-6 ohm/ohm • °F................17
20 – 100°C, µ Ω/Ω• °C ..................................30
Coefficient of Expansion, 68 – 212°F, 10-6 in/in • °F.....8.17
20 – 100°C, µm/m • °C .........14.7
Thermal Conductivity, Btu • in/ft2 • h • °F ...........................155
W/m • °C ..........................................22.4
Electrical Resistivity, ohm • circ mil/ft ...............................295
µ Ω• m ..............................................0.490
TYPICAL MECHANICAL PROPERTIES
(Annealed)
Tensile Strength, ksi ..................................................................60
MPa ............................................................415
Yield Strength (0.5% Offset), ksi ...........................................21
MPa .....................................145
Elongation, % ..............................................................................32
Tensile Strength, ksi ..................................................................60
MPa ............................................................415
Yield Strength (0.5% Offset), ksi ...........................................21
MPa .....................................145
Elongation, % ..............................................................................32