产品名称

INCONEL 690

没有此类产品
产品描述
INCONEL alloy 690 is a high-chromium nickel alloy with excellent resistance to many corrosive aqueous media and high-temperature atmospheres. The alloy's high chromium content gives it excellent resistance to aqueous corrosion
by oxidizing acids (especially nitric acid) and salts, and to sulfidation at high-temperatures.In addition to its corrosion resistance, alloy 690 has high strength, good metallurgical stability and favorable fabrication characteristics.
STANDARD PRODUCT FORMS
Pipe, tube, plate, round bar and forging stock.
MAJOR SPECIFICATIONS
UNS N06690
ASTM B 163, B 166 – B 168,
B 564, B 829
ASME Code Cases 2083,
N-20, N-525
ASME SB-163, SB-166 –
SB-168, SB-564, SB-829
Werkstoff Nr. 2.4642
ISO 6207, 6208, 9723
ISO NW6690
LIMITING CHEMICAL COMPOSITION, %
Nia.........58.0 min.
Cr....... 27.0 – 31.0
Fe.........7.0 – 11.0
C...........0.05 max.
aPlus Co.
Mn........0.50 max.
S........ 0.015 max.
Si..........0.50 max.
Cu........0.50 max.
PHYSICAL CONSTANTS AND THERMAL PROPERTIES
Density, Ib/in3.........................................................................0.296
g/cm3......................................................................... 8.19
Melting Range, °F...................................................2450 – 2510
°C....................................................1343 – 1377
Specific Heat, Btu/lb•°F.....................................................0.107
J/kg•°C............................................................ 450
Permeability at 200 Oersted (15.9 kA/m).....................1.001
Coefficient of Expansion, 10-6 in/in•°F (μm/m•°C)
70-200°F (21–93°C)...................... 7.80 (14.0)
70-1000°F (21–538°C).................8.53 (15.4)
70-1600°F (21–970°C).................9.38 (16.9)
Thermal ConductivityA, Btu•in/ft2•h•°F.....................................84
W/m•°C.............................................. 12.1
Electrical ResistivityA, ohm•circ mil/ft...................................691
μΩ•m...................................................1.15
Young’s ModulusA, 106 psi.................................................... 30.6
GPa........................................................... 211
Poisson’s RatioA....................................................................... 0.29
HardnessA, HRB...........................................................................85
ARoom temperature, as aged.
TYPICAL MECHANICAL PROPERTIES
INCONEL 690
Corresponding parameter set not found, please add it in property template of background
暂未实现,敬请期待
暂未实现,敬请期待